Scenarios
Semiconductors · Semiconductor · CVD DepositionExample scenario

CVD Film Thickness Uniformity

The deposition rate profile shifts with chamber use, but the recipe is corrected only at periodic measurements. Edge thickness deviation builds up in between and costs yield.

−25%Within-wafer thickness non-uniformity
−15%Reworked wafers

Example scenario. Figures are illustrative.

Plant dataWafers since clean1,840
PrescriptionEdge heater temperature550 → 556 ℃
PrescriptionSiH₄ flow200 → 192 sccm
Expected resultThickness non-uniformity4.0% → 3.0%
Plant dataPrescriptionExpected result

On the floor

01
Situation
After 1,200 wafers since the last chamber clean, edge film thickness is 3% thinner than the center.
02
Trade-off
Raising edge temperature narrows the deviation but moves mean thickness off target; leaving it lets uniformity keep degrading.
03
Limit
Engineers correct the recipe by hand after weekly measurement, so wafers in between carry the deviation.

How we solve it

Learns how settings affect thickness profile from heater zone temperatures, gas flow, wafer count and thickness measurements, then calculates zone temperatures and flow within the mean thickness target.

Plant data

  • Heater zone temperatures
  • SiH₄ flow
  • Chamber pressure
  • Wafers since clean
  • Film thickness measurement

Prescription

  • Edge heater temperature550 ℃ → 556 ℃
  • SiH₄ flow200 sccm → 192 sccm
Also adjustedChamber cleaning interval

Constraints

  • Mean thickness within ±2% of target
  • Within heater maximum temperature

Expected results

Within-wafer thickness non-uniformity−25%
4.0%→3.0%
BeforeExpected
Reworked wafers−15%
200 wafers/mo→170 wafers/mo
BeforeExpected

Could this work for your process?

Tell us about your process and data, and we will assess feasibility.

Request a free assessment